As we all know, stone is a natural product, which contains a variety of natural chemicals. These natural chemical substances may be activated and decomposed as long as the chemical properties are under certain conditions, or chemical changes may cause the surface of the stone to be damaged, which greatly affects the decorative effect of the stone. In addition, stone is also extremely susceptible to contamination by external substances. If it is not properly protected on the surface, external dirt is very easy to invade the outer surface and interior of the stone and the stone becomes ugly, thus greatly reducing the ornamental value of the stone. And decorative effects. Following Xiaobian to see the use of water-based stone protection agent .
Water-based stone protection agent
First, plate cleaning
Before construction, be sure to remove oil, dust, and other debris on the surface of the stone and dry the stone. If the stone is not fully dried spraying protective agent, it may cause protection agent failure or appearance abnormal.
Second, process debugging
Prior to construction, a small area of ​​debugging should be carried out to determine the reasonable amount of protective agent and spraying process. If the debugging fails, please seek technical support from the manufacturer and distributor promptly.
Third, the product Kaifeng
Clean the lid before opening (it must be free of water and dust).
After opening, check the appearance of the product. If the product is found to have abnormalities such as foreign objects or turbidity, please suspend use.
Fourth, tool preparation
All protective agent contact tools and containers must be dry, clean, and dedicated. Mixing water-based and oil-based tools can cause protective agent failure or abnormal equipment.
Fifth, spray or soak
The protective agent should be applied uniformly and in sufficient amounts, and the amount of the protective agent should be sufficient to ensure that the surface of the stone is completely wetted and no liquid residue remains on the surface. All six sides of the stone must be painted evenly. If the stone is soaked in a protective agent, the effect is better.
Insufficient spraying may result in partial water seepage; overspray may affect the appearance of the stone, such as white spots or darkening.
After spraying, the stone must be exposed to the sun for more than 2 hours to produce a waterproof effect; if there is no sun, it should be properly extended to dry (or blow dry, dry) time.
Sixth, finished product inspection
Before the sheet is packaged, it should be sampled for splashing water test. Only after passing the test can the board be collected (make sure that the stone protection effect is good before leaving the factory).
Close the bottle cap immediately after use. Prolonged exposure to air may deteriorate the protective agent. Protective agents should be stored in a dry place away from open flames and inaccessible to children.
Stone common disease
1. Bai Hua. A white, gray, grayish black, black mist-like substance that affects the appearance of the stone is created on the surface of the stone. Baihua stone disease often exists in the serpentine green stone. Some white Chinese fabrics can be easily wiped off. Some white Chinese fabrics are very stubborn and must be re-polished.
2, yin and yang face. A watermark (water-stained) created by stones that have been left unused for long periods of time after water intrusion and exposure to moisture.
3, yellow stone surface or produce yellow spots. This type of stone disease is commonly found in white stone materials (such as white linen, white flowers, and white snowflakes) and has always been a major problem in stone surface treatment.
4. Stone is contaminated by oil or other dirt (eg coffee juice, soy sauce, juice, tea, chewing gum).
5. The color of cement or adhesive penetrates from the back of the stone board to the front of the board to change the original color of the stone.
6, moldy.
7, stone surface moss. The stone that was installed in the damp place will produce moss on the stone surface after several years.
8, was corroded by the acid rain in the atmosphere and change the original natural bright stone.
Editor's summary: I'll introduce you to the use of water-based stone protection agent . I hope to help you, and more information on the decoration is on this site. Please stay tuned.
Marble white microcrystalline stone
Fecr Electrode Paste Cylinders